The foil-faced insulation fabric roll has high-temperature thermal stability, durability, and the ability to resist high-temperature shrinkage.
Fiberglass insulation with aluminum backing can maintain safety, stability, and high performance for a long time within the recommended operating temperature range and under normal working conditions while reducing heat loss.
The fibers inside the glass wool are fluffy and interlaced, and there are a lot of tiny pores. It is a typical porous sound-absorbing material and has good sound-absorbing properties.
Tested by European standards EN13162:2012/AC:2005 and BG8624-2012 standards, Heaterk ultra-long microfiber glass wool is a non-combustible grade A material.
Grid Glass Fiber Reinforced Aluminum Foil |
Glass Fiber Reinforced Aluminum Foil |
Tri-directional Fiberglass Mesh |
Glass Fiber Reinforced Ceramic Fiber |
Bold Tri-directional Fiberglass Mesh |
Plain Weave Glass Fiber Reinforced Aluminum Foil |
Safe Use Temperature | -120℃-400℃ |
Thermal Conductivity | ≤0.0.042w/m.h.℃ |
Combustion Performance |
ASTM E84 |
Sound Absorption Coefficient |
1.03 Product Mixing Method 24kg/m200hz |
Bulk Density | 10-72kg/m³ |
Thickness | 25-150mm |
Length | 3m-20m |
Width | 1200mm |
Bulk Density | 24-74kg/m³ |
Fiber Diameter | <8μm |
Centrifugal Glass Wool Felt Bulk Density | 10-32 Kg/m³ |
Thermal Conductivity of Centrifugal Glass Wool Felt | 0.038w/m.h.℃ |
Centrifugal Glass Wool Felt Specifications | Width 1200mm, Length 11mm22mm, Can Be Customized |
Thickness of Centrifugal Glass Wool Felt | 25-150mm |
Incombustibility | UL181 |
Test Weight(kg/m3) |
GB/T 13350-2000 | 10-96 |
Average Fiber Diameter(um) |
GB/T 13350-2000 | 4.0-6.0 |
Hydrophobicity(%) | JISA 9512-2000 | > 98.5 |
Thermal Conductivity(w/m.k) |
GB/T 13350-2000 | 0.045-0.032 |
Sound Absorption Coefficient | GB/J47-83 | 100 |
Maximum Use Temperature(℃) | GB/T 13350-2000 | 410 |